Chapter 5 · Magnetism and Matter

5.10 Hysteresis

The magnetisation of a ferromagnet is not proportional to H. It does not even depend only on the present value of H: it depends on what has happened to the material before. Fig. 5.28 follows a sample of unmagnetised iron, in the core of a solenoid, as the current in the winding, and so H, is taken up, down, reversed and back again.

O to a: as H rises from zero, B grows, slowly at first, then steeply as the domain walls move, and then levels off as the sample is saturated. a to b: as H is brought back to zero, B does not retrace its path. The domains do not all go back to random directions, and at H = 0 a field remains. This is the  Bᵣ, or remanence. b to c: to bring B down to zero, H must be reversed. The size of the reverse intensity needed is the . c to d: a larger reverse H saturates the sample the other way. d to e to f to a: taking H up again traces the lower half of the loop, through −Bᵣ at H = 0, and B = 0 at a positive H equal to the coercivity, back to saturation.

Fig. 5.28 Tracing a hysteresis loop: B in an iron core against the magnetic intensity H, with the domains shown in the inset at each stage. The shape is typical, not to scale.

The closed curve is a loop, from a Greek word for lagging behind: the magnetisation lags behind the intensity that causes it.

Taking a ferromagnet round its loop costs energy. Moving domain walls and turning domains against the material’s internal friction turn work into heat. Using Faraday’s law (Chapter 6), one can show that the work done per unit volume in changing the field by dB is H dB. Adding round the loop, the energy lost per unit volume in one cycle is the area of the B–H loop:

(5.34)

In a transformer or a motor running on alternating current, the iron core is taken round its loop 50 times a second. The per second, the power turned into heat, is

where V is the volume of the core and f the frequency.

Example 5.22

The soft iron core of a transformer has a volume of 2.0 × 10⁻³ m³, and the area of its hysteresis loop is 300 J m⁻³. The core is taken round its loop 50 times a second. Find the power lost as heat in the core, and the energy lost in a day.

Given

Volume V = 2.0 × 10⁻³ m³ Loop area 300 J m⁻³ Frequency f = 50 s⁻¹

Solution

The power is the energy lost per cycle times the number of cycles per second.

A day lasts 86 400 s:

This is why transformer cores are made of a soft material with a thin loop.

Answer

30 W; 2.6 × 10⁶ J (0.72 kWh) a day

5.10.1 Choosing a magnetic material

The shape of the loop decides what a material is good for (Fig. 5.29, Table 5.6).

Fig. 5.29 Hysteresis loops of (a) soft iron and (b) hard steel, with typical values. Note the different scales of H: the coercivity of the steel is about eighty times larger.

need a large retentivity, so that they stay strongly magnetised, and above all a large coercivity, so that stray fields, knocks and heat do not demagnetise them. Hard steel, Alnico, ferrites and alloys of rare-earth metals are used. need a large permeability, so that a modest current gives a strong field, and above all a small coercivity, so that the magnetism goes away when the current is switched off. Soft iron is used. In a closed ring it keeps a sizeable field at H = 0 (Table 5.6), but its coercivity is so small that in a core of any ordinary shape the field of its own ends wipes this out. The cores of transformers and motors are taken round their loops many times a second. They need a large permeability and a thin loop, of small area, to keep the hysteresis loss low. Iron with a little silicon added, rolled into thin insulated sheets, is used.

Table 5.6 Some magnetic materials, with typical values. Retentivities are for a closed ring of the material; the values depend on how it is made and treated.

Material

Retentivity (T)

Coercivity (A m⁻¹)

Soft iron

≈ 1.0

≈ 50

Silicon steel

≈ 1.2

≈ 40

Hard carbon steel

≈ 0.9

≈ 4 × 10³

Alnico

≈ 1.2

≈ 5 × 10⁴

Ferrite (ceramic)

≈ 0.4

≈ 2.5 × 10⁵

Neodymium magnet (NdFeB)

≈ 1.3

≈ 9 × 10⁵

Soft iron and silicon steel go into electromagnets, relays and the cores of transformers and motors. Hard steel once made compass needles and the first permanent magnets. Alnico is used in meters and guitar pickups, ferrites in fridge magnets, loudspeakers and small motors, and neodymium magnets in phone speakers, hard disks and the motors of electric cars and wind turbines.

Did you know?

The strongest permanent magnets

Neodymium–iron–boron magnets were invented in the early 1980s, by Masato Sagawa in Japan and, independently, by John Croat in the United States. They are the strongest permanent magnets made. Their very large coercivity lets them be made thin and small without demagnetising themselves, which made tiny earphones and light, powerful motors possible. Their Curie temperature is only about 585 K, and they lose coercivity as they warm up, so magnets for hot motors have a little dysprosium added.

Check yourself

Which material is best for the core of an electromagnet that is switched on and off often?

Chapter 5 · Magnetism and Matter

5.10 Hysteresis

The magnetisation of a ferromagnet is not proportional to H. It does not even depend only on the present value of H: it depends on what has happened to the material before. Fig. 5.28 follows a sample of unmagnetised iron, in the core of a solenoid, as the current in the winding, and so H, is taken up, down, reversed and back again.

O to a: as H rises from zero, B grows, slowly at first, then steeply as the domain walls move, and then levels off as the sample is saturated. a to b: as H is brought back to zero, B does not retrace its path. The domains do not all go back to random directions, and at H = 0 a field remains. This is the  Bᵣ, or remanence. b to c: to bring B down to zero, H must be reversed. The size of the reverse intensity needed is the . c to d: a larger reverse H saturates the sample the other way. d to e to f to a: taking H up again traces the lower half of the loop, through −Bᵣ at H = 0, and B = 0 at a positive H equal to the coercivity, back to saturation.

Fig. 5.28 Tracing a hysteresis loop: B in an iron core against the magnetic intensity H, with the domains shown in the inset at each stage. The shape is typical, not to scale.

The closed curve is a loop, from a Greek word for lagging behind: the magnetisation lags behind the intensity that causes it.

Taking a ferromagnet round its loop costs energy. Moving domain walls and turning domains against the material’s internal friction turn work into heat. Using Faraday’s law (Chapter 6), one can show that the work done per unit volume in changing the field by dB is H dB. Adding round the loop, the energy lost per unit volume in one cycle is the area of the B–H loop:

(5.34)

In a transformer or a motor running on alternating current, the iron core is taken round its loop 50 times a second. The per second, the power turned into heat, is

where V is the volume of the core and f the frequency.

Example 5.22

The soft iron core of a transformer has a volume of 2.0 × 10⁻³ m³, and the area of its hysteresis loop is 300 J m⁻³. The core is taken round its loop 50 times a second. Find the power lost as heat in the core, and the energy lost in a day.

Given

Volume V = 2.0 × 10⁻³ m³ Loop area 300 J m⁻³ Frequency f = 50 s⁻¹

Solution

The power is the energy lost per cycle times the number of cycles per second.

A day lasts 86 400 s:

This is why transformer cores are made of a soft material with a thin loop.

Answer

30 W; 2.6 × 10⁶ J (0.72 kWh) a day

5.10.1 Choosing a magnetic material

The shape of the loop decides what a material is good for (Fig. 5.29, Table 5.6).

Fig. 5.29 Hysteresis loops of (a) soft iron and (b) hard steel, with typical values. Note the different scales of H: the coercivity of the steel is about eighty times larger.

need a large retentivity, so that they stay strongly magnetised, and above all a large coercivity, so that stray fields, knocks and heat do not demagnetise them. Hard steel, Alnico, ferrites and alloys of rare-earth metals are used. need a large permeability, so that a modest current gives a strong field, and above all a small coercivity, so that the magnetism goes away when the current is switched off. Soft iron is used. In a closed ring it keeps a sizeable field at H = 0 (Table 5.6), but its coercivity is so small that in a core of any ordinary shape the field of its own ends wipes this out. The cores of transformers and motors are taken round their loops many times a second. They need a large permeability and a thin loop, of small area, to keep the hysteresis loss low. Iron with a little silicon added, rolled into thin insulated sheets, is used.

Table 5.6 Some magnetic materials, with typical values. Retentivities are for a closed ring of the material; the values depend on how it is made and treated.

Material

Retentivity (T)

Coercivity (A m⁻¹)

Soft iron

≈ 1.0

≈ 50

Silicon steel

≈ 1.2

≈ 40

Hard carbon steel

≈ 0.9

≈ 4 × 10³

Alnico

≈ 1.2

≈ 5 × 10⁴

Ferrite (ceramic)

≈ 0.4

≈ 2.5 × 10⁵

Neodymium magnet (NdFeB)

≈ 1.3

≈ 9 × 10⁵

Soft iron and silicon steel go into electromagnets, relays and the cores of transformers and motors. Hard steel once made compass needles and the first permanent magnets. Alnico is used in meters and guitar pickups, ferrites in fridge magnets, loudspeakers and small motors, and neodymium magnets in phone speakers, hard disks and the motors of electric cars and wind turbines.

Did you know?

The strongest permanent magnets

Neodymium–iron–boron magnets were invented in the early 1980s, by Masato Sagawa in Japan and, independently, by John Croat in the United States. They are the strongest permanent magnets made. Their very large coercivity lets them be made thin and small without demagnetising themselves, which made tiny earphones and light, powerful motors possible. Their Curie temperature is only about 585 K, and they lose coercivity as they warm up, so magnets for hot motors have a little dysprosium added.

Check yourself

Which material is best for the core of an electromagnet that is switched on and off often?